This is a longstanding standard in flashing slips. Mix thickly and apply to wet or leatherhard. We use it mostly in the wood kiln, but it’s also nice in soda.
Recipe:
Helmar Kaolin ………….. 80
Nepheline Syenite ……. 20

This is a longstanding standard in flashing slips. Mix thickly and apply to wet or leatherhard. We use it mostly in the wood kiln, but it’s also nice in soda.
Recipe:
Helmar Kaolin ………….. 80
Nepheline Syenite ……. 20